oo Ugu Fiican Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Dhuumaha aan Xumaan Lahayn, Sheet, Soo Saaraha Siliga iyo Alaabta |Guojin

Superalloy InconelX-750/ UNS N07750/ AlloyX-750 Dhuumaha aan Xumaan lahayn, Sheet, Silig

Sharaxaad Gaaban:

Darajo u dhiganta:
UNS N07750
DIN W. Nr.2.4669


Faahfaahinta Alaabta

Tags Product

Alaabooyinka la heli karo

Tuubo aan cillad lahayn, Saxan, Ul, Qalab-abuureyaal, Xir-xirayaal, Ku-xidhayaasha Tubooyinka

Heerarka Wax-soo-saarka

Alaabta

ASTM

Baararka iyo Forgings

B 637

Halabuurka Kiimikada

%

Ni

Cr

Fe

C

Mn

Si

S

Ti

Nb+Ta

Al

Co

Cu

Min

70.0

14.0

5.0

2.25

0.70

0.40

Max

17.0

9.0

0.08

1.00

0.50

0.010

2.75

1.20

1.00

1.00

0.50

Guryaha Jirka

Cufnaanta

8.28 g/cm3

dhalaalay

1393-1427 ℃

Inconel X-750 Tilmaamaha

Inconel X-750 alloy inta badan waa superalloy ku salaysan nikkel kaas oo da' ahaan lagu xoojiyay wejiga γ[Ni3(Al, Ti, Nb)].Waxay leedahay iska caabin daxalka wanaagsan iyo iska caabin oksaydh hoos 980 ℃, iyo ka hooseeya 800 ℃ Waxay leedahay iska caabin daxalka sare.Waxay leedahay iska caabin nasasho oo wanaagsan oo ka hooseeya 540 ° C, iyo sidoo kale qaabaynta iyo alxanka wanaagsan.Daawadaan waxaa inta badan loo adeegsadaa soo saarista matoorada diyaaradaha ee ka shaqeeya wax ka hooseeya 800°C una baahan awood sare..Ilaha ayaa sidoo kale loo isticmaali karaa in lagu soo saaro marawaxadaha marawaxadaha marawaxadaha iyo qaybo kale, sida taarikada, xargaha, baararka, alwaaxyada, faraantiga, fiilooyinka, tuubooyinka, iwm.

Inconel X-750 Habka Daawaynta Kulaylka

Habka daaweynta kulaylka xal ee taarikada, strips iyo tuubooyinka ee gobolka sahayda waa 980 ± 15 ℃, qaboojinta hawada.Nidaamka daaweynta kulaylka dhexdhexaadka ah ee qalabka iyo qaybaha, hababka soo socda ayaa loo dooran karaa daaweynta kulaylka.
Annealing: 955~1010℃, biyo qaboojinta.
Xiritaanka qaybaha alxanka ka hor: 980 ℃, 1h.
Nadiifinta cadaadiska qaybaha alxanka: 900 ℃, qoyaan ilaa 2 saacadood.
Ciribtirka cadaadiska cadaadiska: 885 ± 15 ℃, 24h, qaboojinta hawada.

Inconel X-750 La Heli karo Noocyo iyo Tilmaamo

Baararka, alwaaxyada, faraantiga, go'yaal kulul, go'yaal qabow-duuban, fiilooyin, tuubooyin iyo fiilooyinka ayaa lagu bixin karaa cabbirro kala duwan.
Taarikada iyo xariijimaha guud ahaan waa la keenaa ka dib kulaylka ama qabowga duubka, xoqin ama xalinta, qajaarka iyo turxaan bixinta.
Baararka, been-abuurka iyo faraantiga waxaa lagu bixin karaa qaab la sameeyay ama kulul;sidoo kale waxaa lagu siin karaa daawaynta xalinta ka dib been-abuurka;baararka waxaa la keeni karaa xal ka bacdi oo la turxaan bixiyo ama la rogo, waxaana lagu keeni karaa qabow marka amarku u baahan yahay Jiid gobolka meel.
Xadhkaha waxaa lagu bixin karaa xalalka adag;Siligga leh dhexroorka magaca ama dhumucda ka hooseeya 6.35mm, waxay noqon kartaa xal adag oo la keeno naqshad qabow oo ah 50% ilaa 65%;dhexroorka magaca ama dhererka dhinaca ayaa ka weyn 6.35mm.Silig, daawaynta xalka ka dib, waxaa lagu bixiyaa qallafsanaanta sawir-qabow oo aan ka yarayn 30%.Fiilooyinka leh dhexroorka magaca ama dhererka dhinaca oo aan ka badnayn 0.65mm, waxaa lagu siin karaa qallafsanaanta sawir-qabow oo aan ka yarayn 15% ka dib daaweynta xalka sida loo baahan yahay.

Inconel X-750 Goobaha Codsiga

Daawaha waxaa inta badan loo isticmaalaa soo saarida ilaha caleenta iyo ilo gariiradda leh oo leh shuruudo xoog badan iyo iska caabin nasasho ee matoorada hawada ka hooseeya 800°C.Waxa kale oo loo isticmaali karaa in lagu sameeyo qaybo ay ka mid yihiin marawaxadaha marawaxadaha.Noocyada la heli karo waa xaashida, xariijimaha, birta, foornada, giraanta, siliga iyo tuubada.