oo Soo saaraha iyo alaab-qeybiyaha Superalloy ee ugu Fiican625/ UNS N06625/ Aloy625 Soo saarahaGuojin

Superalloy Inconel625/ UNS N06625/ Soo saaraha Alloy625

Sharaxaad Gaaban:

Darajo u dhiganta:
UNS N06625
DIN W. Nr.2.4856


Faahfaahinta Alaabta

Tags Product

Alaabooyinka la heli karo

Tuubo aan cillad lahayn, Saxan, Ul, Qalab-abuureyaal, Xir-xirayaal, Ku-xidhayaasha Tubooyinka

Heerarka Wax-soo-saarka

Alaabta

ASTM

Baar

B 446

Saxan, Sheet iyo Faleemo

B 443, B 906

Tuubo aan xujo lahayn, tuubo

B 444, B 829

Dhuumaha alxanka leh

B 705, B 775

Qalabka alxanka leh

B 704, B 751

Xidhiidhiyayaasha alxanka leh

B 366

Billet iyo baararka been abuurka ah

B 472

Been abuurasho

B 564

Halabuurka Kiimikada

%

Ni

Cr

Mo

Fe

C

Mn

Si

P

S

Co

Nb+Ta

Al

Ti

Min

58.0

20.0

8.0

3.15

Max

23.0

10.0

5.0

0.10

0.50

0.50

0.015

0.015

1.00

4.15

0.40

0.40

Guryaha Jirka

Cufnaanta

8.36g/cm3

dhalaalay

1330-1375 ℃

Inconel 625 Tilmaamaha

1. Iska caabbinta daxalka heersare ah ee warbaahinta kala duwan ee daxalka ee oxidizing iyo dhimista deegaanka
2. Iska caabin aad u wanaagsan oo u diida daxalka iyo daxalka dillaaca, mana soo saari doono dillaaca daxalka chloride ion stress
3. Iska caabbinta daxalka aad u fiican ee aysiidhka inorganic, sida nitric acid, phosphoric acid, sulfuric acid, hydrochloric acid iyo acids isku dhafan ee sulfuric acid iyo hydrochloric acid, iwm.
4. Iska caabin heer sare ah ee daxalka ee xalalka isku dhafan ee kala duwan ee aashitada inorganic
5. Marka heerkulku gaaro 40 ℃, waxay muujin kartaa iska caabin daxalka wanaagsan ee uruurinta kala duwan ee xal hydrochloric acid
6. Shaqayn wanaagsan iyo weldability, ma laha dareen dildilaac ah oo ka dambeeya alxanka
7. Soo saarida shahaadada weelasha cadaadiska leh heerkulka gidaarka -196~450℃
8. Waxaa shaabadeeyey Jaliyada Maraykanka ee Injineerada Daxalka NACE heerka (MR-01-75) si ay ula kulmaan heerka ugu sarreeya VII ee loogu isticmaalo jawiga gaaska dhanaan.

Inconel625 Goobaha Codsiga

Daawaha hoose ee kaarboonka ee la jilciyay oo la shiiday 625 ayaa si weyn loogu isticmaalaa warshadaha geeddi-socodka kiimikada, iyo iska caabbinta daxalka ee wanaagsan iyo xoogga sare ayaa awood u siinaya in loo isticmaalo qayb qaabdhismeed khafiif ah.Alloy 625 waxaa loo isticmaali karaa codsiyada soo gaadhay biyaha badda oo ay ku xiran tahay culeyska farsamada sare.Aagagga codsiga caadiga ah:
1. Qaybaha hababka kiimikaad ee organic ka kooban chlorides, gaar ahaan halka aysiidh chloride kicinta la isticmaalo
2. Dheefshiideyaasha iyo haamaha bleaching ee warshadaha saxarka iyo waraaqaha
3. Taawarka nuugista, kuleyliyaha, gaaska qiiqa birta, marawaxada (huurka), kicinta, leexiyaha iyo qiiqa nidaamka gaaska hawada ka saara
4. Soo saarista qalabka iyo qaybaha loo isticmaalo gaaska dhanaan
5. Aashitada Acetic iyo Acetic anhydride kicinta
6. Sulfuric acid kondenser